PDF(1442 KB)
Performance of Hydraulic Asphalt Concrete with Acidic Aggregates in Severe Cold Regions
YAN Xiao-hu, LI Hai-feng, LI Da-hong, FENG Wei
Journal of Changjiang River Scientific Research Institute ›› 2026, Vol. 43 ›› Issue (3) : 185-191.
PDF(1442 KB)
PDF(1442 KB)
Performance of Hydraulic Asphalt Concrete with Acidic Aggregates in Severe Cold Regions
[Objective] To facilitate the construction of asphalt concrete core walls in the severe cold regions of Western China, this paper undertakes a systematic investigation into the influence of acidic gravel aggregates on the performance characteristics of hydraulic asphalt concrete. [Methods] The research methodology and evaluation framework were strictly guided by two pivotal Chinese technical standards: Test Code for Hydraulic Asphalt Concrete (DL/T 5362-2018) and the more recent Technical Specification for the Application of Acidic Aggregates in Hydraulic Asphalt Concrete (DL/T 5876-2024). The key performance indicators (mechanical properties, deformation behavior, impermeability, and overall durability) of asphalt concrete incorporating crushed gravel aggregates were evaluated through asphalt concrete water stability tests, direct tensile tests, bending tests, pressure-based impermeability tests for dense-graded asphalt concrete, triaxial compression tests, long-term water immersion stability tests, and long-term freeze-thaw splitting tests. [Results] (1) Complex Composition and Durability Challenge: Gravel aggregates typically exhibited a complex mineralogical composition, encompassing alkaline, neutral, and acidic aggregates, with acidic rock types often being predominant. A primary concern identified was the inherently weak interfacial bonding force between asphalt binder and acidic aggregate surfaces. Under prolonged water immersion, this weak bond facilitated a gradual displacement process where water molecules infiltrated and substituted the asphalt at the aggregate interface, leading to stripping or detachment of the asphalt film from the aggregate surface. This mechanism posed a substantial threat to the long-term durability of the asphalt concrete. Consequently, a thorough durability assessment should be required when considering the application of gravel aggregates-based hydraulic asphalt concrete in critical structures. (2) Enhancement Mechanisms via Cement Filler and Anti-Stripping Agents: The study identified effective methods to mitigate the adhesion issue. Metal ions present in cement, such as Ca2+ and Mg2+, engaged in chemical bonding with oxygen atoms within the asphalt. In the mixing process, this interaction promoted a more robust and durable bond between the asphalt and the aggregates. Furthermore, the use of anti-stripping agents was found to be highly beneficial. These agents operated through multiple synergistic mechanisms, including chemical bonding with the aggregate surface, modification of the interfacial properties, and the creation of a physical barrier against water intrusion. Collectively, these actions significantly enhanced both the durability and the mechanical performance of asphalt concrete made with acidic aggregates. Incorporating cement filler alone, or using a combination of cement filler and non-amine anti-stripping agents, effectively strengthened the adhesive bond between the gravel aggregates and the asphalt matrix, thereby markedly improving the durability of the resulting acidic gravel aggregate hydraulic asphalt concrete. (3) Mechanical Behavior and Modeling: Asphalt concrete was recognized as a temperature-sensitive material. Analysis of triaxial test data revealed that the relationship between lateral strain and axial strain approximated a linear relationship. Specifically for the gravel aggregate asphalt concrete studied, its strength demonstrated a well-defined and favorable linear increase with rising confining pressure. The material's strength could be effectively characterized using the parameters of a linear strength model, namely the cohesion and the angle of internal friction. (4) Overall Performance Improvement: Incorporating cement filler or adding non-amine anti-stripping agents substantially improved the comprehensive performance profile of acidic gravel aggregate asphalt concrete. These enhancements directly translated to superior mechanical properties, increased resistance to water-induced damage, and extended long-term durability. [Conclusion] The application of acidic gravel aggregates in the construction of asphalt concrete core wall dams is demonstrated to be technically feasible. Key performance parameters evaluated in this study, including the long-term water immersion stability coefficient, the freeze-thaw cycle splitting tensile strength ratio, and the failure tensile strain, provide a robust theoretical foundation and essential technical support for the engineering application of this material.
severe cold region / asphalt concrete core wall / acidic gravel aggregate / durability of hydraulic asphalt concrete
| [1] |
闫小虎, 姚新华, 王晓军, 等. 土石坝沥青混凝土心墙材料配合比试验研究[J]. 长江科学院院报, 2017, 34(6): 143-148.
传统观念认为水工沥青混凝土防渗结构中,碱性骨料可以与沥青中的表面活性物质产生化学吸附,有很好的黏附性;酸性骨料与沥青主要是物理吸附作用,与沥青的黏附性和耐久性无法保证,在长期浸水作用下,沥青膜易被水逐渐置换而从骨料表面剥离,从而导致结构破坏。奴尔水利枢纽工程坝址区内有丰富的酸性天然砂砾石料,距坝址较近,便于开采,但其附近没有碱性骨料料场。依托奴尔水利枢纽工程,采用人工灰岩骨料及天然砂砾料2种骨料,进行了室内沥青混凝土配合比性能试验研究,提出了级配指数r=0.40、填料F=12%、人工灰岩骨料沥青含量B=6.9%和天然砂砾石骨料沥青含量B=6.0%优选配合比,供设计参考。
(
In impervious structures such as hydraulic asphaltic concrete, alkaline aggregate is generally considered to be of good adhesion resulted from the chemisorption between alkaline aggregate and surface active materials of asphalt; while acidic aggregate could lead to structural damage as asphalt film is easily replaced by water and detached from aggregate under long-term water immersion because the physical adsorption could not guarantee the adhesion and durability of asphalt. By using artificial limestone and natural gravel aggregates, laboratory tests were conducted to research the mix proportion of hydraulic asphalt concrete for Nuer water control project in Xinjiang, which has rich natural acidic gravel aggregate near the dam site but no alkaline aggregate nearby. Optimization of mix proportion is proposed as follows gradation index <i>r</i>=0.40, filler content <i>F</i>=12%, asphalt content <i>B</i>=6.9% for concrete with artificial limestone aggregates, and <i>B</i>=6.0% for concrete with natural gravel aggregates.
|
| [2] |
宁致远, 刘云贺, 孟霄, 等. 水工沥青混凝土直接拉伸力学性能试验研究[J]. 水力发电学报, 2022, 41(1):74-83.
(
|
| [3] |
邓铭江, 于海鸣, 李湘权. 新疆坝工技术进展[J]. 岩土工程学报, 2010, 32(11): 1678-1687.
(
|
| [4] |
黄振伟, 雷明, 张玮鹏. 西藏拉洛水利枢纽沥青混凝土骨料质量评价及料场比选[J]. 长江科学院院报, 2020, 37(9):149-153,159.
沥青混凝土心墙是土石坝的重要结构,骨料、填料等原材料质量对心墙抗渗性、耐久性及适应变形的能力具有决定性影响。以位于西藏自治区日喀则市的拉洛水利枢纽工程为例,初拟2处沥青混凝土人工骨料石料场以资比选,进行了各项质量参数的试验检测,综合考虑各种因素后选定了运距虽然相对较远但质量更好的卡贡灰岩石料场作为料源,确保高原、高寒、高海拔地区沥青混凝土心墙坝的安全。同时,分析、讨论了沥青混凝土用人工骨料原材料岩石质量评价时应注意的若干问题,并提出了解决问题的意见和建议,可供下一步修订相关标准时参考。
(
Asphalt concrete core wall is an important structure of earth rock dam. The quality of raw materials such as aggregate and filler has a decisive influence on the impermeability, durability and deformation adaptability of the core wall. With Laluo water conservancy project in Rikaze city of Tibet Autonomous Region as an example, we compared two artificial aggregate quarries for the asphalt concrete through testing and inpection of multiple quality parameters. After comprehensive consideration of various factors, we selet Kagong limestone yard which is more distant yet boasts better rock quality as the material source to ensure the safety of asphalt concrete core dam in plateau, cold and high altitude areas. Moreover, we analyze and discusse some problems that should be paid attention to in the quality evaluation of raw materials of artificial aggregate for asphalt concrete, and put forward some suggestions to solve the problems for reference in the revision of relevant standards.
|
| [5] |
|
| [6] |
|
| [7] |
马军, 柳莹, 何建新. 天然砾石沥青混凝土心墙水稳定性技术研究[J]. 水利规划与设计, 2021(2): 110-114.
(
|
| [8] |
董芸, 熊泽斌, 王晓军, 等. 天然砂砾石骨料心墙沥青混凝土耐久性试验研究[J]. 人民长江, 2023, 54(4):218-223.
(
|
| [9] |
何建新, 杨武, 杨耀辉, 等. 水泥填料对心墙沥青混凝土长期水稳定性的影响[J]. 水利水电科技进展, 2017, 37(4): 59-62.
(
|
| [10] |
丁朴荣. 水工沥青混凝土骨料级配选择[J]. 西安理工大学学报, 1990, 6(4): 250-258, 309.
(
|
| [11] |
DL/T 5362—2018, 水工沥青混凝土试验规程[S]. 北京: 中国电力出版社, 2018.
(DL/T 5362—2018, Test Code for Hydraulic Asphalt Concrete[S]. Beijing: China Electric Power Press, 2018. (in Chinese))
|
| [12] |
DL/T 5876—2024, 水工沥青混凝土应用酸性骨料技术规范[S]. 北京: 中国电力出版社, 2024.
(DL/T 5876—2024, Technical Specification for Acid Aggregate Used in Hydraulic Asphalt Concrete[S]. Beijing: China Electric Power Press, 2024. (in Chinese))
|
| [13] |
高磊, 张延亿, 李泽发, 等. 温度对沥青混凝土力学性能影响的三轴试验研究[J]. 水力发电学报, 2025, 44(3): 119-127.
(
|
| [14] |
次仁云旦, 王柳江, 扎西顿珠, 等. 温度对水工沥青混凝土强度及剪胀特性的影响试验研究[J]. 长江科学院院报, 2024, 41(1): 190-195.
(
|
| [15] |
王文政. 天然砾石骨料在沥青混凝土心墙中的适用性研究[D]. 乌鲁木齐: 新疆农业大学, 2014.
(
|
| [16] |
游光明, 何建新, 杨海华. 延长浸水时间对心墙沥青混凝土水稳定性能影响分析[J]. 粉煤灰综合利用, 2016, 30(3):11-13.
(
|
| [17] |
熊泽斌, 闫小虎, 董芸. 酸性骨料沥青混凝土耐久性研究[J]. 人民长江, 2023, 54(3): 200-204, 209.
(
|
/
| 〈 |
|
〉 |