摘要

自生体积变形是影响大坝混凝土抗裂能力的重要因素。针对现有全级配大坝混凝土细观建模效率低、网格质量差的问题,提出随机骨料批投放建模方法建立全级配大坝混凝土二维细观分析模型,研究不同自生体积变形、约束条件下混凝土界面过渡区、砂浆基体的应力分布及其演变规律。结果表明:在收缩和膨胀变形作用下,大坝混凝土应力主要集中在砂浆与骨料尖角临近部位和界面过渡区转角区域,四边约束条件下收缩拉应力较单边约束大0.8~1.2 MPa;以最大拉应力作为开裂控制条件时,高抗裂大坝混凝土的自生体积变形应控制为低收缩或微膨胀,变形宜为(-9~11)×10-6

Abstract

[Objective] Autogenous volume deformation is a key factor affecting the cracking resistance of dam concrete; however, its meso-scale mechanism is often neglected in engineering practice. Meso-scale modeling of full-graded dam concrete has long faced challenges of low efficiency and poor mesh quality, particularly in reconciling, within a unified model, the scale disparity between a maximum aggregate size of up to 150 mm and an interfacial transition zone (ITZ) thickness of only about 50 μm, which prevents accurate representation of the true meso-structural characteristics. To address this issue, we propose a random aggregate batch placement method. [Methods] By optimizing the aggregate generation algorithm and introducing an efficient spatial positioning criterion, rapid placement and high-volume simulation of four-graded aggregates were achieved. An adaptively coordinated meshing technique for the interfacial transition zone was combined with local mesh refinement and geometric smoothing at aggregate-mortar interfaces, thereby constructing a two-dimensional meso-scale analytical model of full-graded dam concrete that accurately captured the micrometer-scale interfacial geometry and mechanical properties. Based on this model, the stress distributions and their evolution within the interfacial transition zone and the mortar matrix were systematically investigated under two autogenous volume deformation modes—shrinkage and expansion—and under different constraint conditions, including single-sided and four-sided constraints. [Results] 1) Different autogenous volume deformation modes governed the spatial distribution characteristics of meso-scale stresses. Under autogenous shrinkage, tensile stresses were concentrated in the cement mortar regions adjacent to sharp aggregate corners because the shrinkage of the mortar matrix was restrained by aggregates, with the local stresses reaching 3.6-4.0 MPa, approaching the tensile strength limit of the mortar. In contrast, under micro-expansion deformation, the restriction of expansion by aggregates caused the tensile stress concentration zones to shift to the specimen surface and the corner regions of internal interfacial transition zones, with a significant increase in the stress concentration factor, indicating that the interfaces became the weak links under expansion conditions. 2) Constraint conditions played a critical role in regulating the stress state of concrete. Compared with a single-sided constraint, the four-sided constraint simulating the strong restraint of a dam foundation significantly amplified the adverse effects of shrinkage deformation, with the shrinkage-induced tensile stresses in the cement mortar generally increasing by 0.8-1.2 MPa, and the local tensile stress at interfaces even exceeding 4.0 MPa, resulting in a sharp increase in cracking risk. Under the same constraint conditions, however, the positive effect of micro-expansion deformation was effectively transformed, causing the concrete as a whole to remain in a compressive stress state and thereby significantly enhancing its cracking resistance. 3) Based on the maximum tensile stress criterion and by comprehensively considering the actual tensile strengths of the mortar and the interfacial transition zone, the safe deformation threshold for high crack-resistant concrete was determined. The autogenous volume deformation of full-graded dam concrete should be strictly controlled within the range of -9×10-6 to 11×10-6. In addition, sensitivity analysis further revealed the influence patterns of key parameters. When the elastic modulus ratio between mortar and aggregate varied by ±20%, the elastic moduli of the mortar and aggregate had a significant effect on the maximum tensile stress of the specimen. Therefore, in dam concrete design, attention should be paid to the coordination between the elastic moduli of mortar and aggregates to prevent excessive tensile stresses induced by autogenous or external deformation. Meanwhile, deformation control indices should be dynamically adjusted according to specific constraint conditions. [Conclusion] Adopting a deformation control strategy of “low shrinkage or micro-expansion” and precisely limiting the deformation magnitude within the above threshold range is an effective approach to enhancing the cracking resistance of dam concrete from the perspective of material design. The established meso-scale model and the obtained quantitative conclusions provide direct evidence for performance-based crack resistance design of concrete. They also offer clear guidance for concrete mix proportion design, optimization of expansive agent dosage, and crack control in practical engineering, and provide a reliable analytical approach for in-depth investigation of deformation coordination and cracking evolution mechanisms of dam concrete at the meso-scale.

关键词

大坝混凝土 / 全级配 / 细观开裂风险 / 自生体积变形 / 随机骨料批投放

Key words

dam concrete / full-graded / meso-scale cracking risk / autogenous volume deformation / random aggregate batch placement

引用本文

导出引用
张开来, 李曙光, 李文伟, . 不同自生体积变形大坝全级配混凝土细观开裂风险分析[J]. 长江科学院院报. 2026, 43(3): 209-217 https://doi.org/10.11988/ckyyb.20250044
ZHANG Kai-lai, LI Shu-guang, LI Wen-wei, et al. Meso-scale Cracking Risk Analysis of Full-graded Dam Concrete with Different Autogenous Volume Deformations[J]. Journal of Changjiang River Scientific Research Institute. 2026, 43(3): 209-217 https://doi.org/10.11988/ckyyb.20250044
中图分类号: TV331 (混凝土结构)   

参考文献

[1]
朱伯芳. 大体积混凝土温度应力与温度控制[M]. 北京: 中国电力出版社,1999.
(ZHU Bo-Fang. Thermal Stresses and Temperature Control of Mass Concrete[M]. Beijing: China Electric Power Press, 1999. (in Chinese))
[2]
李行星, 李维炳. 拱坝混凝土自生体积变形试验研究[J]. 水利建设与管理, 2015, 35(8):28-32.
(LI Xing-xing, LI Wei-bing. Research on Arch Dam Concrete Authigenic Volume Deformation Test[J]. Water Conservancy Construction and Management, 2015, 35(8):28-32. (in Chinese))
[3]
李维炳, 李行星. 大坝混凝土的自生体积变形研究与探讨[J]. 粉煤灰, 2012, 24(2): 40-43.
(LI Wei-bing, LI Xing-xing. Study of Autogenous Volume Deformation of Dam Concrete[J]. Coal Ash, 2012, 24(2): 40-43. (in Chinese))
[4]
冯金根, 段亚辉, 向国兴. 混凝土热学特性对泄洪洞衬砌温度和温度应力影响研究[J]. 水电能源科学, 2010, 28(5):82-85,173.
(FENG Jin-gen, DUAN Ya-hui, XIANG Guo-xing. Study on Influence of Concrete Thermal Characteristics on Temperature and Thermal Stress of Lining Concrete of Spillway[J]. Water Resources and Power, 2010, 28(5): 82-85, 173.(in Chinese))
[5]
李文伟, 江敏敏, 向欣, 等. 高寒地区低热水泥混凝土拱坝温控防裂方案[J]. 南水北调与水利科技(中英文), 2024, 22(5): 967-977.
(LI Wen-wei, JIANG Min-min, XIANG Xin, et al. Temperature Control and Crack Prevention Scheme of Low Heat Cement Concrete Arch Dam in High Cold Area[J]. South-to-North Water Transfers and Water Science & Technology, 2024, 22(5): 967-977. (in Chinese))
[6]
郭传科, 王毅, 任超, 等. 白鹤滩大坝中热与低热水泥混凝土温控对比分析[J]. 水利水电快报, 2018, 39(8): 45-48.
(GUO Chuan-ke, WANG Yi, REN Chao, et al. Comparative Analysis of Temperature Control of Medium Heat and Low Heat Cement Concrete in Baihetan Dam[J]. Express Water Resources & Hydropower Information, 2018, 39(8): 45-48. (in Chinese))
[7]
金浏, 李平, 杜修力. 箍筋约束方形混凝土柱轴压强度尺寸效应律[J]. 应用基础与工程科学学报, 2021, 29(4): 986-998.
(JIN Liu, LI Ping, DU Xiu-li. Size Effect Law of Nominal Compressive Strength for Squared Concrete Columns Confined by Stirrups[J]. Journal of Basic Science and Engineering, 2021, 29(4):986-998. (in Chinese))
[8]
李冬, 黄百惠, 王苑佐, 等. 一种考虑裂缝扩展路径的混凝土细观数值模拟方法[J]. 土木工程学报, 2024, 57(3): 30-41.
(LI Dong, HUANG Bai-hui, WANG Yuan-zuo, et al. A Mesoscopic Numerical Simulation Method for Concrete Considering Crack Propagation Path[J]. China Civil Engineering Journal, 2024, 57(3): 30-41. (in Chinese))
[9]
STORA E, BARY B, HE Q C, et al. Modelling and Simulations of the Chemo-mechanical Behaviour of Leached Cement-based Materials Leaching Process and Induced Loss of Stiffness[J]. Cement and Concrete Research, 2009, 39(9): 763-772.
[10]
徐世烺. 混凝土断裂力学[M]. 北京: 科学出版社, 2011.
(XU Shi-lang. Mechanics of Concrete Fracture[M]. Beijing: Science Press, 2011. (in Chinese))
[11]
邱永荣. 混凝土硬化损伤的细观模拟方法研究与应用[D]. 北京: 清华大学, 2017.
(QIU Yong-rong. Research and Application of Mesoscopic Simulation Method of Concrete Hardening Damage[D]. Beijing: Tsinghua University, 2017. (in Chinese))
[12]
BAŽANT Z P. Size Effect in Blunt Fracture: Concrete, Rock, Metal[J]. Journal of Engineering Mechanics, 1984, 110(4): 518-535.
[13]
GRASSL P, GRÉGOIRE D, ROJAS SOLANO L, et al. Meso-scale Modelling of the Size Effect on the Fracture Process Zone of Concrete[J]. International Journal of Solids and Structures, 2012, 49(13): 1818-1827.
[14]
GRASSL P, JIRÁSEK M. Meso-scale Approach to Modelling the Fracture Process Zone of Concrete Subjected to Uniaxial Tension[J]. International Journal of Solids and Structures, 2010, 47(7/8): 957-968.
[15]
唐欣薇, 张楚汉. 基于均匀化理论的混凝土宏细观力学特性研究[J]. 计算力学学报, 2009, 26(6):876-881.
(TANG Xin-wei, ZHANG Chu-han. Study on Concrete in Macro-and Meso-scale Mechanical Properties Based on Homogenization Theory[J]. Chinese Journal of Computational Mechanics, 2009, 26(6):876-881. (in Chinese))
[16]
马怀发, 陈厚群, 吴建平, 等. 大坝混凝土三维细观力学数值模型研究[J]. 计算力学学报, 2008, 25(2):241-247.
(MA Huai-fa, CHEN Hou-qun, WU Jian-ping, et al. Study on Numerical Algorithm of 3D Meso-mechanics Model of Dam Concrete[J]. Chinese Journal of Computational Mechanics, 2008, 25(2): 241-247. (in Chinese))
[17]
马怀发, 陈厚群, 周永发, 等. 大坝混凝土试件三维细观力学并行计算研究[J]. 工程力学, 2007, 24(10): 74-79.
(MA Huai-fa, CHEN Hou-qun, ZHOU Yong-fa, et al. Parallel Computation Study on 3D Meso-mechanics of Dam Concrete[J]. Engineering Mechanics, 2007, 24(10): 74-79. (in Chinese))
[18]
秦川, 张楚汉. 基于细观力学的混凝土劈拉破坏率相关特性研究[J]. 岩土力学, 2010, 31(12):3771-3777,3783.
(QIN Chuan, ZHANG Chu-han. Study of Dynamic Behavior of Concrete under Splitting Tensile Tests Based on Meso-mechanics[J]. Rock and Soil Mechanics, 2010, 31(12): 3771-3777, 3783.(in Chinese))
[19]
秦川, 郭长青, 张楚汉. 基于背景网格的混凝土细观力学预处理方法[J]. 水利学报, 2011, 42(8):941-948.
(QIN Chuan, GUO Chang-qing, ZHANG Chu-han. A Pre-processing Scheme Based on Background Grid Approach for Meso-concrete Mechanics[J]. Journal of Hydraulic Engineering, 2011, 42(8): 941-948. (in Chinese))
[20]
杜修力, 金浏. 细观分析方法在混凝土物理/力学性质研究方面的应用[J]. 水利学报, 2016, 47(3): 355-371.
(DU Xiu-li, JIN Liu. Applications of Meso-scale Analysis Methods on the Study of the Physical/Mechanical Properties of Concrete[J]. Journal of Hydraulic Engineering, 2016, 47(3): 355-371. (in Chinese))
[21]
杜修力, 金浏. 混凝土静态力学性能的细观力学方法述评[J]. 力学进展, 2011, 41(4):411-426.
(DU Xiu-li, JIN Liu. A Review on Meso-mechanical Method for Studying the Static-mechanical Properties of Concrete[J]. Advances in Mechanics, 2011, 41(4):411-426. (in Chinese))
[22]
XU Y, XU Q, CHEN S, et al. Self-restraint Thermal Stress in Early-age Concrete Samples and Its Evaluation[J]. Construction and Building Materials, 2017, 134: 104-115.
[23]
XU Y, CHEN S. A Method for Modeling the Damage Behavior of Concrete with a Three-phase Mesostructure[J]. Construction and Building Materials, 2016, 102: 26-38.
[24]
GUPTA M, IGARASHI G, TAKAHASHI Y, et al. Multiscale Expansion Modeling of Concrete with Free Lime-based Expansive Additives under Isotropic Conditions Using Poromechanics[J]. Journal of Building Engineering, 2023, 77: 107554.
[25]
李曙光, 李庆斌. 混凝土二维干缩开裂分析的改进弥散裂纹模型[J]. 工程力学, 2011, 28(12): 65-71.
(LI Shu-guang, LI Qing-bin. Two Dimensional Analysis of Drying Shrinkage Micro-cracking in Concrete with Modified Smeared Cracking Model[J]. Engineering Mechanics, 2011, 28(12): 65-71. (in Chinese))
[26]
李曙光. 数字混凝土CT建立方法及其在干缩微裂纹模拟中的应用[D]. 北京: 清华大学, 2010.
(LI Shu-guang. Three Dimensional Simulation of Drying Shrinkage Micro-cracking in Numerical Concrete Reconstructed from CT Images[D]. Beijing: Tsinghua University, 2010. (in Chinese))
[27]
库马尔·梅塔, 保罗·蒙蒂罗.混凝土微观结构、 性能和材料[M]. 欧阳东译. 北京: 中国建筑工业出版社, 2016.
(KUMAR M, PAULO M. Concrete:Microstructure, Properties, and Materials[M]. Translated by OUYANGDong. Beijing: China Architecture & Building Press, 2016. (in Chinese))
[28]
王宗敏. 不均质材料(混凝土)裂隙扩展及宏观计算强度与变形[D]. 北京: 清华大学, 1996.
(WANG Zong-min. Non-homogeneous Materials (Concrete) Crack Propagation and Macroscopic Calculation of Strength and Deformation[D]. Beijing: Tsinghua University, 1996. (in Chinese))
[29]
LEITE J P B, SLOWIK V, MIHASHI H. Computer Simulation of Fracture Processes of Concrete Using Mesolevel Models of Lattice Structures[J]. Cement and Concrete Research, 2004, 34(6): 1025-1033.
[30]
STANKOWSKI T. Numerical Simulation of Progressive Failure in Particle Composites[D]. United States: University of Colorado at Boulder, 1990.
[31]
CABALLERO A, LÓPEZ C M, CAROL I. 3D Meso-structural Analysis of Concrete Specimensunder Uniaxial Tension[J]. Computer Methods in Applied Mechanics and Engineering, 2006, 195(52): 7182-7195.
[32]
韩峰, 徐磊, 金永苗, 等. 混凝土MAZARS本构模型在ABAQUS中的数值实现及验证[J]. 水力发电, 2020, 46(5):85-88,98.
(HAN Feng, XU Lei, JIN Yong-miao, et al. Numerical Implementation and Validation of Concrete MAZARS Constitutive Model in ABAQUS[J]. Water Power, 2020, 46(5): 85-88, 98.(in Chinese))
[33]
李杰, 任晓丹. 混凝土静力与动力损伤本构模型研究进展述评[J]. 力学进展, 2010, 40(3): 284-297.
(LI Jie, REN Xiao-dan. A Review on the Constitutive Model for Static and Dynamic Damage of Concrete[J]. Advances in Mechanics, 2010, 40(3): 284-297. (in Chinese))
[34]
金浏, 籍一丁, 李冬, 等. CFRP布加固RC柱细观力学分析模型及抗扭分析[J]. 北京工业大学学报, 2024, 50(11): 1339-1349.
(JIN Liu, JI Yi-ding, LI Dong, et al. Meso-scale Mechanical Analysis Model of CFRP Sheet-reinforced RC Columns and Torsional Analysis[J]. Journal of Beijing University of Technology, 2024, 50(11): 1339-1349. (in Chinese))
[35]
李文伟, 张超然, 张曙光, 等. 乌东德高拱坝低热硅酸盐水泥混凝土温控防裂和高效施工关键技术技术报告[R]. 武汉: 中国长江三峡集团有限公司, 2020.
(LI Wen-wei, ZHANG Chao-ran, ZHANG Shu-guang, et al, Technical Report on Key Technologies for Temperature Control and Crack Prevention in Low-Heat Portland Cement Concrete and Efficient Construction of the Wudongde High Arch Dam[R]. Wuhan: China Three Gorges Corporation, 2020. (in Chinese))

基金

国家自然科学基金长江联合基金重点项目(U2040222)
湖北省自然科学基金三峡联合基金培育项目(2023AFD196)
湖北省科技创新人才计划项目(2024DJA036)
河南省引江济淮科研服务项目(HNYJJH/JS/FWKY-2021005)

编辑: 任坤杰
PDF(4841 KB)

Accesses

Citation

Detail

段落导航
相关文章

/